Covestro 3741-2-136 UV Cure Secondary Coating (10Kg)
3741-2-136-10KG
Covestro 3741-2-136 UV Cure Secondary Coating (10Kg)
Optical fiber secondary coating.
Product Benefits
Product Benefits
- Industry-standard
- Fast cure
- Compatible with wet-on-wet or wet-on-dry coating process
- Compatible with multiple DeSolite primaries
- Patent-protected
- Viscosity, 25°C, 4,750 mPa•s
- Viscosity, 35°C, 2,050 mPa•s
- Density, 23°C, 1121 kg•m-3
- Liquid Refractive Index, 23°C, 1.519
- Surface tension, 23°C, 24 dynes•cm-1
- Segment modulus, 2.5% strain, 731 MPa
- Elongation, 27%
- Tensile strength, 29 MPa
- Degree of Cure (UV dose at 95% of Ultimate Secant Modulus, J•cm-2 ): 0.2
- Dynamic water sensitivity (150 µm films)
- peak absorption, 1.6%
- extractables, 0.8%
- Hydrogen generation (24 hrs, 80°C in air, 75 µm films, µl•g-1): 0.2
- Volumetric coefficient of expansion (DMA), 500 µm films
- in the glassy region (x10-6), <100°C-1
- in the rubbery region (x10-6), 450°C-1
- Refractive Index: 1.537
- Aging after 8 weeks Thermal weight change,
- 3% at 95°C
- 3% at 125°C
- Glass Transition Range (DMA), 29°C at E’ 1000 MPa
- Glass Transition Range (DMA), 51°C at E’ 100 MPa